The key points of heat treatment of aluminum extrusion die

1. The quality of heat treatment of aluminum extrusion die directly affects the service life of the extrusion die. Quenching is to improve the hardness of the mold, and repeated tempering is to improve the toughness of the mold and stabilize the internal structure. The hardness value of mold heat treatment is specified: large aluminum extrusion die (F>500mm), HRC45-48; Múnla meánach (F300 ~ 500mm), HRC47-50; Bás easbhrúite beag (f<300mm), HRC48-51; Three points are tested on the same plane of a set of molds, and the hardness value of each point should be qualified within the specified range.

 

2. Ba chóir aird ar leith a thabhairt ar roinnt pointí sa phróiseas cóireála teasa maidir le heasnamh easbhrúite bás:

a. Ba chóir go mbeadh luas teasa na rannóige teochta ard - go tapa, agus níor chóir go mbeadh an t -am gabháltas ró -fhada, chun cosc ​​a chur ar an easbhrúite bás ó róthéamh nó róthéamh, róthéamh - grán garbh, róthéamh - eilimintí pointe leá íseal a bheith ina gcúis le héagsúlacht;

b. Tar éis an mhúchadh, ba cheart an bás easbhrúite alúmanaim a mhaolú in am chun scoilteanna a chosc;

c. Nuair a fhaightear go bhfuil cruas an easbhrúite bás neamhleor nó míchothrom tar éis cóireála teasa, ba chóir anáil a dhéanamh, agus ba chóir an chóireáil teasa a athdhéanamh de réir an phróisis (nuair a bhíonn an luach cruas
d. Maidir le múnlaí móra easbhrúite alúmanaim nó múnlaí críochnaithe le cuasa casta, ba chóir próiseas faoisimh strus - a chur leis (chun deireadh a chur le próiseáil leictreach agus strus meaisínithe, is é sin, chun strus teirmeach agus strus microstruchtúir a dhíothú);

 

E. Ba chóir go mbeadh teocht ola múchta an mhúnla 100 céim chun an éifeacht múchta a chinntiú.